When design engineers and decision makers at OEMs or supplier programs are contemplating aluminum die casting, the baseline question is bound to appear. High pressure vs low pressure die casting, which is right for me?

Both forms of die casting utilize reusable dies to make quality aluminum parts. Where they differ is how the dies are filled, ultimately proving that processes are best for different parts. Before answering the question, it’s critical to consider wall thickness, part size, production volume, costs, and more.

General Die Casters breaks down both high pressure vs low pressure die casting and ultimately which one is best for your program’s needs.

How High Pressure Die Casting Works

The high pressure die casting process commonly features six critical steps: preparation/clamping, transfer, injection, cooling, ejection, and finishing operations.

Steel dies house the part cavity and ultimately where the liquified metal will flow too. Before this occurs, the die needs temperature conditioned and lubricated. After this, the two halves are closed and clamped together for resistance.

Nowadays, automation transfers a specified amount of molten material from the furnace into the shot sleeve where the injection into the die occurs. Once the injection happens, the steel die draws heat out of the material quickly and pressure is maintained to support cooling. After proper cooling has occurred, the die is opened and the cast part is ejected from the mold. Any trimming, finishing operations, and secondary operations take place and once finished, the part is done.

How Low Pressure Die Casting Works

Low-pressure die casting also has its own set of operations, but the key differences lie in how the molten material finds the die. The aluminum and the die still need prepared as they do in high-pressure operations. The differences start to take noticeable effect after preparation. In low-pressure die casting, the die is situated above a sealed furnace that already contains the melted material. A tube connecting the material and the die is how the material travels into the die rather than being injected like in high-pressure die casting.

Pressure is maintained throughout the cooling process until the casted part has solidified and then pressure is released. From there, the part is finished.

HPDC vs LPDC: Key Differences

Factor High-Pressure Die Casting Low-Pressure Die Casting
How the die fills A piston forces metal into the cavity at high speeds and pressure Gas pressure in a sealed furnace pushes metal upward through a riser tube into the cavity
Pressure ranges 1000-25,000 PSI depending on the process and application 4-21 PSI with room for interpretation and room to move outside of these ranges
Production speed Fast filling and short cycles, commonly used for high volumes Slower filling and longer cycles
Wall thickness and detail Best suited for thin walls, fine features, and complex external shapes Requires thicker walls
Porosity tendency Rapid, turbulent filling creates a larger risk of trapped gas Gentler filling reduces gas entrapment, and controlled feeding helps produce adequate castings
Surface finish and accuracy Strong surface finish and dimensional repeatability Offers good surface finish and dimensional accuracy, but thin-feature capability is more limited
Internal passages and cores Relies on retractable metal cores Can accommodate sand cores for more flexibility for complex internal passages
Equipment and tooling More complex injection and clamping equipment Simpler equipment and lower clamping requirements
Material utilization Runners, gates, and overflows contribute to metal that must be trimmed High material utilization is possible

When High Pressure Die Casting Is the Right Choice

  • Medium- to high-volume programs where piece price matters
    • Higher tooling cost is offset by long tool life, with die cavities generally handling at least 100,000 cycles
    • Multi-cavity dies lower part price
  • Thin-walled, complex, lightweight parts with tight tolerances
  • Parts needing a surface finish ready for blasting, painting, anodizing, plating, or polishing
  • Parts that need to be heat treated or pressure tight
    • Vacuum assist, specialty alloys, and good process control can reduce porosity
    • Applications: housings, brackets, valve and actuator bodies, EV components

When Low Pressure Die Casting May Fit Better

  • Lower volumes, or larger, thicker-walled parts
  • Structural parts where density and strength come first, such as wheels and suspension arms

Partner with General Die Casters for Custom High Pressure Die Castings

General Die Casters is one of the country’s most experienced high pressure aluminum die casting manufacturers. Since 1957, our Northeast Ohio facility has served OEMs, supplier programs, and more with custom solutions backed by robust quality management systems and dedicated customer service.

We specialize in high pressure operations for our customers’ parts because of the many aforementioned benefits, but also because of the alloys we can supply. We’re located in between Cleveland and Akron, in Twinsburg, Ohio, where our complete die casting capabilities are housed. Not only do we perform the die casting process, but we also offer CNC machining, heat treatment, finishing operations, pressure testing, and light assembly.